How to solve the spots problem during blister packaging production?


baby shoe tree


(1) The surface finish of the mold cavity is too high

Air is trapped on the smooth mold surface, causing acne spots on the surface of the product. The surface of the cavity should be sandblasted, and additional vacuum holes can be added.


(2) Poor pumping

Air extraction holes should be added. If the acne occurs only in a certain part, check whether the suction hole is blocked or add a suction hole in the area.


(3) The mold temperature is too high or too low

Should be adjusted appropriately. If the mold temperature is too high, the cooling should be strengthened and the mold temperature should be lowered; if the mold temperature is too low, the mold temperature should be increased and the mold should be insulated.


(4) Improper selection of mold material

When processing transparent sheets, do not use phenolic resin to make molds, but use aluminum molds.


(5) The mold surface is too rough

The surface of the cavity should be polished to improve the surface finish.


(6) The surface of the sheet or mold cavity is not clean

The dirt on the surface of the sheet or cavity should be completely removed.


(7) There are scratch marks on the surface of the sheet

The surface of the sheet should be polished, and the sheet should be stored with paper.


(8) The dust content of the air in the production environment is too high

The production environment should be purified.


(9) The mold draft is too small

Should be increased appropriately.